Item 200 Aggregate Subbase Course

16 questions • 2026-01-10
Anonymous
Report

Question

According to AASHTO T89, the fraction passing the No. 40 sieve (0.425mm) shall have a LL of:

  • not greater than 25

  • not greater than 35

  • Skip

Question

According to AASHTO T90, the fraction passing the No. 40 sieve (0.425mm) shall have a PI of:

  • not greater than 12

  • not greater than 6

  • Skip

Question

When the required thickness is more than ______, the aggregate subbase shall be spread and compacted into ______ or more layers of approximately equal thickness, and the minimum compacted thickness of any layer shall not exceed ______.

Answer

Question

Compaction on each layer shall continue until a the FDT result is _____.

Answer

Question

At least _____ in situ FDT should be conducted in trial section of _____ or fraction thereof per material or procedure and per layer

Answer

Question

Permitted variation from design thickness of layer

  • +/- 10mm

  • +/- 20mm

  • Skip

Question

Permissible variation in design level of surface

  • +10mm/-20mm

  • +5mm/-10mm

  • Skip

Question

Permitted surface irregularity measured by 3m straight edge

  • 5mm

  • 20mm

  • Skip

Question

Permitted variation from design crossfall or camber

  • +/- 0.1%

  • +/- 0.3%

  • Skip

Question

Permitted variation from design longitudinal grade over 25m in length

  • +/- 0.3%

  • +/- 0.1%

  • Skip

Item 200 Aggregate Subbase Course

TestMaker

Score

0 / 10

Correct rate

0%

Correct: 0

Incorrect: 0

Unanswered: 10

 
ankimaker.com

Question list

  • 1

    According to AASHTO T89, the fraction passing the No. 40 sieve (0.425mm) shall have a LL of:

    not greater than 35

  • 2

    According to AASHTO T90, the fraction passing the No. 40 sieve (0.425mm) shall have a PI of:

    not greater than 12

  • 3

    When the required thickness is more than ______, the aggregate subbase shall be spread and compacted into ______ or more layers of approximately equal thickness, and the minimum compacted thickness of any layer shall not exceed ______.

    150mm, two, 150mm

  • 4

    Compaction on each layer shall continue until a the FDT result is _____.

    100%

  • 5

    At least _____ in situ FDT should be conducted in trial section of _____ or fraction thereof per material or procedure and per layer

    three, 500sq.m

  • 6

    Permitted variation from design thickness of layer

    +/- 20mm

  • 7

    Permissible variation in design level of surface

    +10mm/-20mm

  • 8

    Permitted surface irregularity measured by 3m straight edge

    20mm

  • 9

    Permitted variation from design crossfall or camber

    +/- 0.3%

  • 10

    Permitted variation from design longitudinal grade over 25m in length

    +/- 0.1%

  • 11

    Basis of payment is in _____.

    cubic meter

  • 12

    The course portion, retained on a No. 40 sieve (2mm) shall have a mass percent of wear ___ max by the Los Angeles Abrasion Test

    50%

  • 13

    The material shall have a soaked CBR value of ___ max as determined by AASHTO T193

    30%

  • 14

    Laboratory Compaction Test and Quality Test for every:

    1500cu.m

  • 15

    Grading Test and Plasticity Test (LL, PL, PI) for every:

    300cu.m

  • 16

    California Bearing Ratio (CBR) Test for every:

    2500cu.m