    Where is information found concerning acceptable species substitution for wood materials used in aircraft repair?

    AC 43. 13-B

  • 2

    Which of the following conditions will determine acceptance of wood with mineral streaks?

    Careful inspection fails to reveal any decay

  • 3

    Compression failures in wood aircraft structures are characterized by buckling of the fibers that appear as streaks on the surface

    At right angles to the grain

  • 4

    Which statement concerning wood decays is correct?

    Any form or amount of decay is not permitted

  • 5

    In cases of elongated boltholes in a wood spar or cracks in the vicinity of boltholes,

    A new section of spar should be spliced in or the spar replaced entirely

  • 6

    Glue deterioration in wood aircraft structure is indicated

    When a joint has separated and the glue surface shows only the imprint of the wood with no wood fibers clinging to the glue

  • 7

    The I-beam wooden spar is routed to

    Reduce weight

  • 8

    Pin knot clusters are permitted in wood aircraft structure provided

    They produce a small effect on grain direction

  • 9

    Which statement about wood decay is correct?

    Decays is not acceptable in any form or amount

  • 10

    Any wooden member that has been overstretched is subject to which type of failure?

    Compression failure

  • 11

    The cantilever wing uses

    No external bracing

  • 12

    Laminated wood is sometimes used in the construction of highly stressed aircraft components. This wood can be identified by its

    Parallel grain construction

  • 13

    Laminated wood spars may be substituted for solid rectangular wood spars

    If the same quality wood is used in both

  • 14

    A faint line running across the grain of a wood spar generally indicates

    Compression Failure

  • 15

    When patching a plywood skin, abrupt changes in cross-sectional areas which will develop dangerous stress concentration should be avoided by using

    Circular or elliptical patches

  • 16

    The strength of a well-designed and properly prepared wood splice joint is provided by the

    Glue

  • Airframe Aircraft Finishes

    Airframe Aircraft Finishes

    AR Ramos · 15問 · 1年前

    Airframe Aircraft Finishes

    Airframe Aircraft Finishes

    15問 • 1年前
    AR Ramos

    Airframe Aircraft Covering

    Airframe Aircraft Covering

    AR Ramos · 12問 · 1年前

    Airframe Aircraft Covering

    Airframe Aircraft Covering

    12問 • 1年前
    AR Ramos

    Airframe Ice & Rain Control Systems

    Airframe Ice & Rain Control Systems

    AR Ramos · 28問 · 1年前

    Airframe Ice & Rain Control Systems

    Airframe Ice & Rain Control Systems

    28問 • 1年前
    AR Ramos

    Aircraft Fire Extinguishing System

    Aircraft Fire Extinguishing System

    AR Ramos · 30問 · 1年前

    Aircraft Fire Extinguishing System

    Aircraft Fire Extinguishing System

    30問 • 1年前
    AR Ramos

    Airframe Aircraft Position And Warning System

    Airframe Aircraft Position And Warning System

    AR Ramos · 35問 · 1年前

    Airframe Aircraft Position And Warning System

    Airframe Aircraft Position And Warning System

    35問 • 1年前
    AR Ramos

    Aircraft Maintenance Ground Operation & Servicing

    Aircraft Maintenance Ground Operation & Servicing

    AR Ramos · 38問 · 1年前

    Aircraft Maintenance Ground Operation & Servicing

    Aircraft Maintenance Ground Operation & Servicing

    38問 • 1年前
    AR Ramos

    Aircraft Maintenance Fluid Lines & Fitting

    Aircraft Maintenance Fluid Lines & Fitting

    AR Ramos · 35問 · 1年前

    Aircraft Maintenance Fluid Lines & Fitting

    Aircraft Maintenance Fluid Lines & Fitting

    35問 • 1年前
    AR Ramos

    Aicraft Maintenance Engine Inspection

    Aicraft Maintenance Engine Inspection

    AR Ramos · 29問 · 1年前

    Aicraft Maintenance Engine Inspection

    Aicraft Maintenance Engine Inspection

    29問 • 1年前
    AR Ramos

    Aircraft Maintenance Cleaning & Corrosion Control

    Aircraft Maintenance Cleaning & Corrosion Control

    AR Ramos · 34問 · 1年前

    Aircraft Maintenance Cleaning & Corrosion Control

    Aircraft Maintenance Cleaning & Corrosion Control

    34問 • 1年前
    AR Ramos

    問題一覧

  • 1

    Where is information found concerning acceptable species substitution for wood materials used in aircraft repair?

    AC 43. 13-B

  • 2

    Which of the following conditions will determine acceptance of wood with mineral streaks?

    Careful inspection fails to reveal any decay

  • 3

    Compression failures in wood aircraft structures are characterized by buckling of the fibers that appear as streaks on the surface

    At right angles to the grain

  • 4

    Which statement concerning wood decays is correct?

    Any form or amount of decay is not permitted

  • 5

    In cases of elongated boltholes in a wood spar or cracks in the vicinity of boltholes,

    A new section of spar should be spliced in or the spar replaced entirely

  • 6

    Glue deterioration in wood aircraft structure is indicated

    When a joint has separated and the glue surface shows only the imprint of the wood with no wood fibers clinging to the glue

  • 7

    The I-beam wooden spar is routed to

    Reduce weight

  • 8

    Pin knot clusters are permitted in wood aircraft structure provided

    They produce a small effect on grain direction

  • 9

    Which statement about wood decay is correct?

    Decays is not acceptable in any form or amount

  • 10

    Any wooden member that has been overstretched is subject to which type of failure?

    Compression failure

  • 11

    The cantilever wing uses

    No external bracing

  • 12

    Laminated wood is sometimes used in the construction of highly stressed aircraft components. This wood can be identified by its

    Parallel grain construction

  • 13

    Laminated wood spars may be substituted for solid rectangular wood spars

    If the same quality wood is used in both

  • 14

    A faint line running across the grain of a wood spar generally indicates

    Compression Failure

  • 15

    When patching a plywood skin, abrupt changes in cross-sectional areas which will develop dangerous stress concentration should be avoided by using

    Circular or elliptical patches

  • 16

    The strength of a well-designed and properly prepared wood splice joint is provided by the

    Glue