問題一覧
1
flat and horizontal positions
2
CC and CV
3
100%
4
true
5
it minimizes arc blow with multiple wire set-ups
6
the wire electrode will slip and feed erratically
7
the weld will be flashing and will likely result in porosity
8
the space between two unrestrained loops of wire
9
knurled or V-groove
10
constant speed
11
increase arc voltage
12
wider arc stream and shallower penetration
13
when shallower penetration is required
14
1.6 mm to 6.4 mm (1/16" to 1/4")
15
CSA uses the metric system to measure tensile strength values.
16
active flux
17
fused
18
they should be dried or rebaked according to manufacturer specifications.
19
yes
20
no
100 official format practice questions.
100 official format practice questions.
Fern Hiebert · 100問 · 1年前100 official format practice questions.
100 official format practice questions.
100問 • 1年前SMAW Fillet Welds on Mild Steel
SMAW Fillet Welds on Mild Steel
Fern Hiebert · 25問 · 1年前SMAW Fillet Welds on Mild Steel
SMAW Fillet Welds on Mild Steel
25問 • 1年前SMAW and Oxyfuel Cutting on Mild Steel
SMAW and Oxyfuel Cutting on Mild Steel
Fern Hiebert · 23問 · 1年前SMAW and Oxyfuel Cutting on Mild Steel
SMAW and Oxyfuel Cutting on Mild Steel
23問 • 1年前SMAW Groove Welds on Mild Steel
SMAW Groove Welds on Mild Steel
Fern Hiebert · 20問 · 1年前SMAW Groove Welds on Mild Steel
SMAW Groove Welds on Mild Steel
20問 • 1年前GTAW Equipment Maintenance and troubleshooting
GTAW Equipment Maintenance and troubleshooting
Fern Hiebert · 31問 · 1年前GTAW Equipment Maintenance and troubleshooting
GTAW Equipment Maintenance and troubleshooting
31問 • 1年前GTAW Electrodes Filler Metals and Shielding Gases
GTAW Electrodes Filler Metals and Shielding Gases
Fern Hiebert · 28問 · 1年前GTAW Electrodes Filler Metals and Shielding Gases
GTAW Electrodes Filler Metals and Shielding Gases
28問 • 1年前Distortion
Distortion
Fern Hiebert · 23問 · 1年前Distortion
Distortion
23問 • 1年前Layout
Layout
Fern Hiebert · 9問 · 1年前Layout
Layout
9問 • 1年前GMAW on Mild Steel
GMAW on Mild Steel
Fern Hiebert · 19問 · 1年前GMAW on Mild Steel
GMAW on Mild Steel
19問 • 1年前FCAW and MCAW on Mild Steel
FCAW and MCAW on Mild Steel
Fern Hiebert · 13問 · 1年前FCAW and MCAW on Mild Steel
FCAW and MCAW on Mild Steel
13問 • 1年前The GTAW Process
The GTAW Process
Fern Hiebert · 29問 · 1年前The GTAW Process
The GTAW Process
29問 • 1年前2. 100 official format practice questions
2. 100 official format practice questions
Fern Hiebert · 62問 · 1年前2. 100 official format practice questions
2. 100 official format practice questions
62問 • 1年前GMAW FCAW & MCAW Groove Welds on Mild Steel
GMAW FCAW & MCAW Groove Welds on Mild Steel
Fern Hiebert · 8問 · 1年前GMAW FCAW & MCAW Groove Welds on Mild Steel
GMAW FCAW & MCAW Groove Welds on Mild Steel
8問 • 1年前Pattern Development
Pattern Development
Fern Hiebert · 15問 · 1年前Pattern Development
Pattern Development
15問 • 1年前Metallurgy for Practical Applications
Metallurgy for Practical Applications
Fern Hiebert · 16問 · 1年前Metallurgy for Practical Applications
Metallurgy for Practical Applications
16問 • 1年前Nickel Alloys and Clad Steels
Nickel Alloys and Clad Steels
Fern Hiebert · 9問 · 1年前Nickel Alloys and Clad Steels
Nickel Alloys and Clad Steels
9問 • 1年前Codes and Standards Part A & B
Codes and Standards Part A & B
Fern Hiebert · 31問 · 1年前Codes and Standards Part A & B
Codes and Standards Part A & B
31問 • 1年前Metal Identification
Metal Identification
Fern Hiebert · 32問 · 1年前Metal Identification
Metal Identification
32問 • 1年前問題一覧
1
flat and horizontal positions
2
CC and CV
3
100%
4
true
5
it minimizes arc blow with multiple wire set-ups
6
the wire electrode will slip and feed erratically
7
the weld will be flashing and will likely result in porosity
8
the space between two unrestrained loops of wire
9
knurled or V-groove
10
constant speed
11
increase arc voltage
12
wider arc stream and shallower penetration
13
when shallower penetration is required
14
1.6 mm to 6.4 mm (1/16" to 1/4")
15
CSA uses the metric system to measure tensile strength values.
16
active flux
17
fused
18
they should be dried or rebaked according to manufacturer specifications.
19
yes
20
no